If you keep your boat at a dock with the shore power cabled plugged in, you should have one of these devices to prevent galvanic corrosion.
Posts Tagged ‘galvanic corrosion’
Keep Aluminum and Brass Separated in the Marine Environment
August 18th 2012
Thread sealer alone won't keep these two metals apart, and they're far enough from each other on the galvanic scale for corrosion to occur if exposed to seawater.
Thread sealer alone won't keep these two metals apart, and they're far enough from each other on the galvanic scale for corrosion to occur if exposed to seawater.
Boat Wiring: Shorepower Mystery Box
September 22nd 2011
The white box connected to the shorepower grounding wire is a galvanic insulator, Ed Sherman explains.
The white box connected to the shorepower grounding wire is a galvanic insulator, Ed Sherman explains.